The stringer didn't flatten out, which I was surprised. I took the temp up to 1450, but I didn't hold it.


The texture stayed where I applied the second layer of stringer. Next phase is to slump.

Manual Firing Schedule:
Note: Starting temp in kiln - 85 deg

Lo for 60 min.
At 60 min, temp=670, turned up to L2
At 1:30, temp=900, turn up to L3
At 2:00, temp=1050, turn up to L4
At 2:20, temp=1240, turn up to L5
At 2:30, temp=1330, turn up to L6
At 2:42, temp=1450
Turn kiln off and let cool overnight.